18
Stress test
Resistance to soldering heat
Thermal shock
ESD
Solderability
Specification and acceptance criteria
X7R
∆C/C within ±4.5%
∆C/C within ±7.5% for 25 V
D.F. < 25 · 10
D.F. < 50 · 10
I.R. > 1 · 10
(whichever is less)
-
∆C/C within ±4.5%
∆C/C within ±7.5% for 25 V
D.F. < 25 · 10
D.F. < 50 · 10
I.R. > 1 · 10
(whichever is less)
Covering of 95% of end terminations, checked by visual
inspection. No leaching of contacts.
5
5
MΩ or τ > 1000 s resp. 500 s for 25 V
MΩ or τ > 1000 s resp. 500 s for 25 V
-3
-3
-3
-3
for 25 V
for 25 V
Page 10 of 14
MLSC 0805, 50 V and 100 V
Test description in
accordance to AEC-Q200
Immerse the MLCC in and eutectic
solder at 260 ±5 °C for 10 ±1 s,
measurements 24 ±2 h after test @
room temperature
Covered by more severe tests No. 4
Test setup and performance as per
AEC-Q200-002.
Note: Test and classification only for
information. For ESD protection the
use of MLV is recommended.
Conditions:
a)
b)
c)
for 4 h, immerse the MLCC in
eutectic solder (60/40 SnPb) at
235 °C ±5 °C for 5 +0/-0.5 s.
aging for 8 h ± 15 min, immerse
the MLCC in eutectic solder (60/40
SnPb) at 235 °C ±5 °C for 5 +0/-
0.5 s.
aging for 8 h ±15 min, immerse
the MLCC in eutectic solder (60/40
SnPb) at 260 °C ±5 °C for 120 ±5
s.
Preconditioning at 155 °C
Preconditioning by steam
Preconditioning by steam